Supply OEM/ODM 3 * 7mmpp/PE/PVC Plastic Electrode for Plastic Welding

Short Description:

J556 (AWS E8016-G) is a low alloy steel electrode with low hydrogen potassium type coating. Both AC and DC can be used, and can be welded in all positions.


Product Detail

Product Tags

Reliable good quality and very good credit standing are our principles, which will help us at a top-ranking position. Adhering to your tenet of “quality 1st, purchaser supreme” for Supply OEM/ODM 3 * 7mmpp/PE/PVC Plastic Electrode for Plastic Welding, We give priority to quality and customer satisfaction and for this we follow stringent quality control measures. We have in-house testing facilities where our products are tested on every aspect at different processing stages. Owning to latest technologies, we facilitate our customers with customized production facility.
Reliable good quality and very good credit standing are our principles, which will help us at a top-ranking position. Adhering to your tenet of “quality 1st, purchaser supreme” for China Welding Rods and Polyethylene Rod, The products and solutions has a good reputation with competitive price, unique creation, leading the industry trends. The company insists on the principle of win-win idea, has establishedglobal sales network and after-sales service network.
APPLICATIONS:

Welding of 9% Cr-1% Mo steels and 9% Cr – 2% Mo steels used for electric power and high pressure vessel.

DESCRIPTIONS:

PA-8016-B8 is a low hydrogen electrode whose weld metal consists of 9%Cr-1%Mo. It is designed for high temperature steel and steels for hot hydrogen services, particularly in petrochemical industry. The electrode can be approved for its high tensile strength, good toughness and great heat resistance.

NOTES ON USAGE:

1. Dry the electrodes at 350-400°C for about one hour before use and store the electrodes at 100-150°C after drying them with attention to keep away from moisture.

2. Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose to prevent blowholes at the arc starting.

3. Keep the arc as short as possible.

4. Preheat at 100-150°C. The temperature to be applied varies in accordance with plate thickness and kind of steel to be welded.

5. Pay attention not to exceed proper heat-input because excessive heat-input causes deterioration of impact values and yield strength of weld metal.

IV. TYPICAL CHEMICAL COMPOSITION OF WELD METAL (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. TYPICAL MECHANICAL PROPERTIES OF WELD METAL:

Tensile Strength N/mm2 (Ksi)

Yield Point N/mm2

(Ksi)

Elongation %

PWHT

705 (102)

560 (81)

24

740°C x 1 hr

VI. WELDING POSITIONS: ALL POSITIONS

VII. SIZE AND RECOMMENDED CURRENT RANGE (AC/DC+):

Diameter (mm)

2.5

3.2

4.0

5.0

Length (mm)

350

350

400

400

Ampere

Flat

55 – 85

90 – 130

130 – 180

180 – 240

V & OH

50 – 80

80 – 115

110 – 170

150 – 200

Reliable good quality and very good credit standing are our principles, which will help us at a top-ranking position. Adhering to your tenet of “quality 1st, purchaser supreme” for Supply OEM/ODM 3 * 7mmpp/PE/PVC Plastic Electrode for Plastic Welding, We give priority to quality and customer satisfaction and for this we follow stringent quality control measures. We have in-house testing facilities where our products are tested on every aspect at different processing stages. Owning to latest technologies, we facilitate our customers with customized production facility.