AWS A5.4 E309L-16 Stainless Steel Welding Rods Best Welding Electrode

Short Description:

A062 (AWS E309L-16) is an ultra-low carbon Cr23Ni13 stainless steel electrode with titanium-calcium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A062                                         

GB/T E309L-16

AWS E309L-16                

Description: A062 is an ultra-low carbon Cr23Ni13 stainless steel electrode with titanium-calcium coating. It can be used for both AC and DC. It has a low carbon content, so it can resist intergranular corrosion caused by carbide precipitation without stabilizers such as niobium and titanium.

Application: It is used for the same type of stainless steel structure, composite steel, and special-shaped steel components in the manufacture of synthetic fiber, petrochemical, and other equipment. It can also be used for the surfacing of transition layers on the inner wall of nuclear reactor pressure vessels and the welding of tower internals.

 

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 70

80 ~ 110

130 ~ 160

160 ~ 200

 

Notice:

1. The electrode must be baked for 1 hour at around 150℃ before welding operation;

2. Because the penetration depth is shallow during AC welding, the DC power supply should be used as much as possible to get deeper penetration. and the current should not be too large to avoid redness of the welding rod

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

OEM/ODM:

We support OEM/ODM and could make packaging accord to your design, please contact us for detail discussion.


  • Previous:
  • Next: