Stainless Steel Arc Welding Rods AWS A5.4 E310H-16 Best Quality Welding Electrode Supplier

Short Description:

A432 (AWS A5.4 E310H-16) is a 3Cr26Ni21 heat-resistant stainless steel electrode with titanium-calcium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A432                                 

GB/T E310H-16

AWS A5.4 E310H-16

Description: A432 is a 3Cr26Ni21 heat-resistant stainless steel electrode with titanium-calcium coating. It can be used for both AC and DC with excellent operating performance. The deposited metal has high creep strength, good joint performance, and low thermal crack sensitivity.

Application: It is specially used for welding HK40 heat-resistant steel.

 

 Chemical composition of weld metal(%):

C

Cr

Ni

Mo

Mn

Si

Cu

S

P

0.35 ~ 0.45

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

1.0 ~ 2.5

≤0.75

≤0.75

≤0.030

≤0.030

 

 Mechanical properties of weld metal:

Test item

 

Tensile strength

Mpa

Elongation

%

Guaranteed

≥620

≥10

 

 Recommended current:

Rod diameter

(mm)

3.2

4.0

5.0

Welding Current

(A)

80 ~ 110

110 ~ 160

160 ~ 200

 

Notice:

  1. The electrode must be baked for 1 hour at around 150℃ before welding operation;
  2. Because the penetration depth is shallow during AC welding, the DC power supply should be used as  much as possible to get deeper penetration. and the current should not be too large to avoid redness of the welding rod.

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 