Nickel Alloy Welding Wire ERNiCr-3 Nickel Tig Wire Filler Metal

Short Description:

Alloy 82 (ERNiCr-3 ) is used for the welding of alloys 600, 601, 690, 800 and 800HT etc.


Product Detail

Product Tags

Nickel Alloy Welding WireTig Wire ERNiCr-3

Standards
EN ISO 18274 – Ni 6082 – NiCr20Mn3Nb
AWS A5.14 – ER NiCr-3

 

Features and Applications

Alloy 82 is used for the welding of alloys 600, 601, 690, 800 and 800HT etc.

Weld metal deposited has high strength and good corrosion resistance, including oxidation resistance and creep rupture strength at elevated temperatures.

Ideal for dissimilar welding applications between various nickel alloys, stainless steels, carbon steels including overlay.

Suitable for applications ranging from cryogenic to high temperatures making this alloy one of the most used in the nickel family.

Typically used in the power generation and petrochemical industries etc.

Typical Base Materials

Alloy 600, Alloy 601, Alloy 690, Alloy 800, Alloy 330*
* Illustrative, not exhaustive list

 

 

Chemical Composition %

C%

Mn%

Fe%

P%

S%

Si%

 

max

2.50

max

max

max

max

 

0.05

3.50

3.00

0.030

0.015

0.50

 

 

Cu%

Ni%

Co%

Ti%

Cr%

Nb+Ta%

 

max

67.00

max

max

18.00

2.00

 

0.50

min

1.00

0.75

22.00

3.00

 

 

Mechanical Properties
Tensile Strength ≥600 MPa  
Yield Strength ≥360 MPa  
Elongation ≥30 MPa  
Impact Strength ≥100 MPa  

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

 

Shielding Gases

EN ISO 14175 – TIG: I1 (Argon)

 

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

Packaging Data
Diameter Length Weight  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 Kg

5 Kg

 

 

Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained, this information is subject to change without notice and can be only considered as suitable for general guidance.