Nickel Alloy Welding Wire ERNiCrCoMo-1 Nickel Tig Wire Filler Metal

Short Description:

Alloy 617 (ERNiCrCoMo-1) is a high temperature wire used for welding of nickel-chromium-cobalt-molybdenum alloys.


Product Detail

Product Tags

Nickel Alloy Welding WireTig Wire ERNiCrCoMo-1

 

Standards
EN ISO 18274 – Ni 6617 – NiCr22Co12Mo9
AWS A5.14 – ER NiCrCoMo-1

 

Features and Applications

Alloy 617 is a high temperature wire used for welding of nickel-chromium-cobalt-molybdenum alloys.

Ideal for overlay cladding where similar alloy is required, such as gas turbines and ethylene equipment.

Suitable for joining dissimilar alloys where high temperature strength and oxidation resistance are required up to about 1150°C.

Typically used in the aerospace and power generation industries, including petrochemical plants for applications such as nitric acid catalyst grids etc.

Typical Base Materials

Inconel alloys 600 and 601, Incoloy alloys 800 HT and 802 and cast alloys such as HK40, HP and HP45 Modified. UNS Number N06617, 2.4663, 1.4952, 1.4958, 1.4959, NiCr21Co12Mo, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, Alloy 617, N08810, N08811*
* Illustrative, not exhaustive list

 

 

Chemical Composition %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

0.05

max

max

max

max

max

max

0.10

1.00

1.00

0.020

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Mo%

44.00

10.00

0.80

max

20.00

8.00

min

14.00

1.50

0.60

24.00

10.00

 

Mechanical Properties
Tensile Strength ≥620 MPa
Yield Strength -
Elongation -
Impact Strength -

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

 

Shielding Gases

EN ISO 14175 – TIG: I1 (Argon)

 

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

Packaging Data

Diameter

Length

Weight

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 