Nickel Alloy Welding Wire ENiFe-Cl Mig Welding Wire

Short Description:

Ferro-nickel solid wire used for welding cast iron and ductile iron.


Product Detail

Product Tags

Nickel Alloy Welding Wire ENiFe-Cl

Features and Applications

Ferro-nickel solid wire used for welding cast iron and ductile iron.

Suitable for dissimilar joints between cast iron, mild steel, low alloy and stainless steels.

Recommended for welding high sulphur, phosphorous or lubricant-contaminated castings.

Precision layer wound for superior wire feeding characteristics.

Typically used for a range of repair and fabrication applications, including rebuilding shafts, wheels, critical joints between steel and cast iron etc

Typical Base Materials

Grey cast iron, malleable, nodular*
* Illustrative, not exhaustive list

 

Standards
EN ISO 1071 – SC NiFe-1
AWS A5.15 – E NiFe-CI

 

Chemical Composition %
C% Mn% Si% P% S%
max max max max max
2.00 0.80 0.20 0.03 0.03
Fe% Ni% Cu% Al%
rem. 54.00 max max
56.00 2.50 1.00

 

Mechanical Properties
Tensile Strength 400 – 579 MPa
Yield Strength -
Elongation -
Impact Strength -

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

 

Shielding Gases

EN ISO 14175 – I1, Ar + 1-2% O2

 

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF

 

Packaging Data
Diameter
Weight Spool Pallet Qty
1.20 mm 15 Kg BS300 72