Hot Selling for Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode

Short Description:

J556 (AWS E8016-G) is a low alloy steel electrode with low hydrogen potassium type coating. Both AC and DC can be used, and can be welded in all positions.


Product Detail

Product Tags

Adhering for the theory of “quality, services, performance and growth”, we have received trusts and praises from domestic and worldwide shopper for Hot Selling for Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode, We hope we can have a friendly relationship with businessman from all over the world.
Adhering for the theory of “quality, services, performance and growth”, we have received trusts and praises from domestic and worldwide shopper for China E7018 Welding Electrode and Welding Electrode E7018, We welcome an opportunity to do business with you and hope to have pleasure in attaching further details of our products and solutions. Excellent quality, competitive price, punctual delivery and dependable service can be guaranteed. For further inquires please do not hesitate to contact us.
APPLICATIONS:

Welding of 9% Cr-1% Mo steels and 9% Cr – 2% Mo steels used for electric power and high pressure vessel.

DESCRIPTIONS:

PA-8016-B8 is a low hydrogen electrode whose weld metal consists of 9%Cr-1%Mo. It is designed for high temperature steel and steels for hot hydrogen services, particularly in petrochemical industry. The electrode can be approved for its high tensile strength, good toughness and great heat resistance.

NOTES ON USAGE:

1. Dry the electrodes at 350-400°C for about one hour before use and store the electrodes at 100-150°C after drying them with attention to keep away from moisture.

2. Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose to prevent blowholes at the arc starting.

3. Keep the arc as short as possible.

4. Preheat at 100-150°C. The temperature to be applied varies in accordance with plate thickness and kind of steel to be welded.

5. Pay attention not to exceed proper heat-input because excessive heat-input causes deterioration of impact values and yield strength of weld metal.

IV. TYPICAL CHEMICAL COMPOSITION OF WELD METAL (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. TYPICAL MECHANICAL PROPERTIES OF WELD METAL:

Tensile Strength N/mm2 (Ksi)

Yield Point N/mm2

(Ksi)

Elongation %

PWHT

705 (102)

560 (81)

24

740°C x 1 hr

VI. WELDING POSITIONS: ALL POSITIONS

VII. SIZE AND RECOMMENDED CURRENT RANGE (AC/DC+):

Diameter (mm)

2.5

3.2

4.0

5.0

Length (mm)

350

350

400

400

Ampere

Flat

55 – 85

90 – 130

130 – 180

180 – 240

V & OH

50 – 80

80 – 115

110 – 170

150 – 200

Adhering for the theory of “quality, services, performance and growth”, we have received trusts and praises from domestic and worldwide shopper for Hot Selling for Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode, We hope we can have a friendly relationship with businessman from all over the world.
Hot Selling for China E7018 Welding Electrode and Welding Electrode E7018, We welcome an opportunity to do business with you and hope to have pleasure in attaching further details of our products and solutions. Excellent quality, competitive price, punctual delivery and dependable service can be guaranteed. For further inquires please do not hesitate to contact us.