Hardfacing Welding Electrodes DIN 8555 (E1-UM-350) Surfacing Welding Rods, Wear Resistant Stick Electrode

Short Description:

DIN 8555 (E1-UM-350) is a basic coated SMAW electrode for crack and wear resistant surfacing.


Product Detail

Product Tags

Hardfacing Welding Electrode

 

Standard: DIN 8555 (E1-UM-350)

Type No.: TY-C DUR 350

 

Specification & Application:

· Basic coated SMAW electrode for crack and wear resistant surfacing.

· Good abrasion resistance. Easy to weld in all positions.

· Particularly suited for wear resistant surfacing on Mn-Cr-V alloyed parts, such as frogs, track rollers, chain support rolls, sprocket wheels, guide rolls etc.

 

Chemical composition of deposited metal(%):            

 

C

Si

Mn

Cr

Fe

DIN

-

-

-

-

-

EN

-

-

-

-

-

Typical

0.20

1.2

1.40

1.8

Bal.

 

 

Hardness of deposited metal:

As Welded

(HB)

1 layer on steel with C=0.5%

(HB)

370

420

 

General Characteristics:   

· Microstructure      Ferrite + Martensitic

· Machinability       Good with Tungsten carbides tipped tools

· Preheating         Preheat heavy parts and higher-tensile steels to 250-350℃

· Redrying           Redry for 2 h at 300℃ before using.

 


  • Previous: