D132 (B-83) Hardfacing Welding Electrode, Surfacing Welding Rod, Arc Welding Stick

Short Description:

Low hydrogen electrode for reconstruction welds. Welds can be machined (turned, planed, milled, etc.). High compressive strength. Good resistance to moderate abrasion.


Product Detail

Product Tags

Hardfacing Welding Stick ElectrodeRODO P

RODO PARA RECUBRIMIENTO PROTECTOR

Type No.: B – 83

Deposited Metal Analysis (Typical values)

C

0.1%

Mn

0.9%

Si

0.8%

Cr

3.2%

 

Characteristics:

Low hydrogen electrode for reconstruction welds. Welds can be machined (turned, planed, milled, etc.). High compressive strength. Good resistance to moderate abrasion.

 

Mechanical Properties: Hardness 27-31 HRc

 

Welding Positions: Flat, Horizontal, Overhead, Vertical Up.

 

Current and Polarity:

For alternating or direct current

electrode to positive pole

ø mm

ø in

Amperage

3.20

1/8

110-130

4.00

5/32

140-180

5.00

2/16

190-240

 

Applications: In feed rollers, pulleys, brake shoes.

• To fill sprockets of tractors

• Excellent as a base for hard coatings on carbon steels.

carbon

• Trunnions, axles and caterpillars of mechanical shovels.

• Crusher cylinders

• Conveyor rollers

 

 

LENGTH: 350mm.

WEIGHT PER BOX: 20 kg/44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 


  • Previous:
  • Next: