G202 Stainless Steel Welding Electrode, GB/T E410-16 Welding Rods for All Positions

Short Description:

G202 (GB/T E410-16 ) is a Cr13 stainless steel electrode with titanium calcium coating. It can be used for all-position welding with AC and DC.


Product Detail

Product Tags

Stainless Steel Welding Electrode

G202                                                         

GB/T E410-16                   

Description: G202 is a Cr13 stainless steel electrode with titanium calcium coating. It can be used for all-position welding with AC and DC.   

Application: Used for welding 06Cr13 and 12Cr13 stainless steel structures, and can also be used for corrosion-resistant and wear-resistant surface surfacing. 

 Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0. 12

≤1.0

≤0.90

11.0 ~ 13.5

≤0.7

≤0.75

≤0.75

≤0.03

≤0.04

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Elongation

%

Guaranteed

≥450

≥20

 

Recommended current:

Rod diameter

(mm)

3.2

4.0

5.0

Welding Current

(A)

80 ~ 120

100 ~ 160

150 ~ 200

Notice:

1. The electrode must be baked for 1 hour at around 150℃ before welding operation;

2. The weldment must be preheated to 250 ~ 350°C before welding.

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 