Flux Cored Arc Welding Wire AWS A5.22 E309LMoT1-1 Stainless Steel Wire

Short Description:

AWS A5.22 E309LMoT1-1 Flux Cored Arc Welding Wire is a modified type of 309L with the addition of molybdenum.


Product Detail

Product Tags

Flux Cored Arc Welding Wire AWS A5.22 E309LMoT1-1

EN ISO 17633-A-T 23 12LPC1 1

Characteristics and Application
AWS A5.22 E309LMoT1-1 Flux Cored Arc Welding Wire is a modified type of 309L with the addition of molybdenum. It is
suitable for joining stainless steels to unalloyed steels. The addition of molybdenum enhances creep strenght and
improves corrosion resistance.

Typical chemical Composition of Weld Metal (%)
C 0.025 Mn1.16 Si0.57 P 0.023 S 0.007 Cr 23.46 Ni 12.51 Mo 2.20

Typical Mechanical Properties of Weld Metal
Tensile Strenght 685MPa Elongation 33%

Notes on usage:
1. Before welding, oil, rusty, and moisture should be cleaned off the base material that should have the proper
protection from the wind in welding site.
2. Use 99.8% or higher purity Co2 as shielding gas.Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.