ENiFe-CI Nickel Alloy Welding Wire, FN 55 Nickel Tig Wire Ferro-nickel Solid Wire

Short Description:

Ferro-nickel solid wire used for welding cast iron and ductile iron.


Product Detail

Product Tags

Nickel Alloy Welding Wire Tig Wire ENiFe-CI

Standards
EN ISO 1071 – SC NiFe-1
AWS A5.15 – E NiFe-CI

 

Features and Applications

Ferro-nickel solid wire used for welding cast iron and ductile iron.

Suitable for dissimilar joints between cast iron, mild steel, low alloy and stainless steels.

Recommended for welding high sulphur, phosphorous or lubricant-contaminated castings.

Typically used for a range of repair and fabrication applications, including rebuilding shafts, wheels, critical joints between steel and cast iron etc.

Typical Base Materials

Grey cast iron, malleable, nodular*
* Illustrative, not exhaustive list

 

Chemical Composition %

C%

Mn%

Si%

P%

S%

   

max

max

max

max

max

   

2.00

0.80

0.20

0.03

0.03

   

   

Fe%

Ni%

Cu%

Al%

   

rem.

54.00

max

max

   

56.00

2.50

1.00

   

 

Mechanical Properties
Tensile Strength 400 – 579 MPa  
Yield Strength -  
Elongation -  
Impact Strength -  

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

 

Shielding Gases

EN ISO 14175 – TIG: I1 (Argon)

 

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF

 

Packaging Data

Diameter

Length

Weight

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg