E71T-1C/1M-PLUS A5.20, Carbon Steel Flux Cored Arc Welding Electrodes Mig Welding Wire

Short Description:

E71T-GS is a carbon steel, a flux-cored electrode for use without an external shielding gas.  This electrode is intended for welding thin-gauge carbon steel, ranging from 3/16” to 22 gauge.


Product Detail

Product Tags

E71T-GS is a carbon steel, flux-cored electrode for use without an external shielding gas.  This electrode is intended for welding thin-gauge carbon steel, ranging from 3/16” to 22 gauge.

Typical Applications:  single-pass weldments; this product is designed to weld quite effectively over galvanized material and can  be used on certain aluminized surfaces as well.  E71T-GS requires no external gas-shielding and should be welded with DCEN (straight polarity).

AWS Class: E71T-GS Certification:   AWS A5.20/A5.20M:2005
Alloy:  E71T-GS AWS/ASME SFA A5.20

 

Welding Position:
H, F, V, O
Current:
DCEN
Straight Polarity

 

Transverse Tensile Strength, kpsi: 86.4min (Base metal fracture)
Guided Bend Test Meets AWS requirements

 

Typical Wire Parameters
Diameter Process Amps Volts Wire Feed Speed
in (mm)
.030″ 0.8 FCAW 50 15 80
    FCAW 100 16 225
    FCAW 150 17 375
    FCAW 175 17 445
.035″ 0.9 FCAW 75 15 70
    FCAW 100 16 110
    FCAW 150 17 180
    FCAW 200 18 305
.045″ 1.2 FCAW 100 15 70
    FCAW 150 16 120
    FCAW 200 17 195
    FCAW 225 17 245
1/6″ 1.6 FCAW 150 17 60
    FCAW 200 18 85
    FCAW 250 18 135
    FCAW 300 19 180
5/64”  .078 FCAW 200 19 60
    FCAW 250 20 80
    FCAW 300 21 115
    FCAW 325 120 6.6

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.