E308L-17 Stainless Steel Welding Rod

Short Description:

E308L-17 For Stainless Steel Welding Electrode Welding Rod (Low C, 18%Cr- 8%Ni)


Product Detail

Product Tags

E308L-17 For Stainless Steel Welding Electrode Welding Rod (Low C, 18%Cr- 8%Ni)

Classifications

EN IS03581-A:2016: E 19 9 L R 12

EN IS03581-B:2016: ES308L-17

AWS A5.4-2014: E308L-17

JISZ 3221-2013 : ES308L-17

Description

-Covering is lime titania type for welding of 18%Cr-8%Ni stainless steel. (AISI 301, 302, 304, 308)

-Excellent welding dfficiency because of high deposition rate.

-Remove Water, rust, oil and all foreign matters from the groove prior to welding.

-Good usability with direct current applications.

-Preheating is not necessary in general.

-Redry the electrode at 250~350°C for 30~60 minutes prior to use.

Chemical Composition Deposited Metal (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Sizes & Recommended Current (AC or DC)
Welding rod diameter
(mm)
2.5 3.2 4.0 5.0
welding current
(A)
55-80 90-130 110-150 140-180

Characteristics on Usage:

Very stable arc.

Excellent removability of slag.

Penetration is shallow.

Good heat and corrosion resistance.

Excellent crack resistance.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for 22 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes and other welding accessories & consumables.