E2209T1-1/T1-4 Stainless Steel Flux Cored Welding Wire

Short Description:

It is optimized for positional welding, both vertical up and for fixed pipework qualified in the ASME 5G or 6G welding positions (pipe typically > 150mm diameter, > 15mm wall).
Smooth all position weldability


Product Detail

Product Tags

AWS Class E2209T1-1/T1-4 Flux Core Wire

FEATURES 
Is optimized for positional welding, both vertical up and for fixed pipework qualified in the ASME 5G or 6G welding positions (pipe typically > 150mm diameter, > 15mm wall).
Smooth all position weldability
Excellent slag removal

Shielding Gas
80% Argon / 20% CO2
100% CO2

Key Features
• Smooth all position weldability
• Vacuum sealed pack
• Excellent slag removal
• Certificate showing deposit composition, ferrite number, and charpy impact properties tested @ -196°C (-320°F)

AWS Class E2209T1-1/T1-4 Flux Core Wire Chemical Composition

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
AWS Class E2209T1-1/T1-4 Flux Core Wire Mechanical Properties
Tensile Strength 120,000 psi
Yield Strength 95,000 psi
Elongation (%) 26%
AWS Class E2209T1-1/T1-4 Flux Core Wire Parameters
  Diameter   WFS (ipm)   Amperage   Volts   ESO (in.) Deposition Rate
(lbs/hr)
  .045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
  1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.