DIN 8555 (E6-UM-60) Hard Surfacing Welding Rod, Wear Resistant Welding Electrode Arc Stick Electrode

Short Description:

DIN 8555  (E6-UM-60) is a basic coated SMAW electrode for hard surfacing  with excellent resistance against compression stresses and impacts.


Product Detail

Product Tags

Hardfacing Welding Electrode

 

Standard: DIN 8555  (E6-UM-60)

Type No.: TY-C DUR 600

 

Specification & Application:

· Basic coated SMAW electrode for hard surfacing.

· Excellent resistance against compression stresses and impacts.

· Universally applicable for cladding on parts of steel, cast steel and high Mn-steel, subject simultaneously to abrasion, impact and compression. Typical application fields are the earth moving and stone treatment industry, e.g. excavator teeth, bucket knives, crusher jaws and cones, mill hammers etc.

 

 Chemical composition of deposited metal(%):      

 

C

Si

Mn

Cr

Mo

Nb

Ni

W

V

Fe

DIN

0.2

2.0

-

-

5.0

-

-

-

-

-

-

Bal.

EN

0.2

2.0

-

0.3

3.0

5.0

18.0

-

4.5

-

10

-

-

2.0

-

2.0

Bal.

Typical

0.50

2.3

1.80

9.0

-

-

-

-

-

Bal.

 

 

Hardness of deposited metal:

As Welded

(HRC)

After soft-annealing 780-820℃/oven

(HRC)

After hardening 1000-1050℃/oil

(HRC)

1 layer on

high Mn-steel

(HRC)

2 layer on

high Mn-steel

(HRC)

56 – 58

25

60

22

40

 

General Characteristics:   

· Microstructure      Martensitic

· Machinability       Good with Tungsten carbides tipped tools

· Preheating         Preheat heavy parts and higher-tensile steels to 200-350℃

· Redrying           Redry for 2 h at 300℃ before using.


  • Previous: