Carbon Steel Welding Electrode AWS A5.1 E7024 Arc Stick Electrode

Short Description:

J501Fe18 (AWS E7024) is an iron powder titanium-type high-efficiency carbon steel electrode.


Product Detail

Product Tags

Carbon Steel Welding Electrode

J501Fe18                                                        

GB/T E5024

AWS A5.1 E7024   

Description: J501Fe18 is an iron powder titanium-type high-efficiency carbon steel electrode. The deposition efficiency is around 180%, which is suitable for flat welding and flat fillet welding.

Application:  It is used for the welding of low carbon steel, general strength hull structural steel ClassA, Class B and high strength hull structural steel AH32, AH36.

 

Chemical composition of weld metal(%):

C

Mn

Si

S

P

≤0.12  

≤1.25

≤0.60

≤0.035

≤0.035

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

(0℃)

Guaranteed

≥490

≥400

≥23

≥47

X-ray inspection:   II grade

 

Recommended current:

Rod diameter

(mm)

3.2

4.0

5.0

5.6

6.0

Welding current

(A)

130 ~ 170

180 ~ 230

250 ~ 340

280 ~ 400

300 ~ 430

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 


  • Previous:
  • Next: