AWS/ASME 5.3 E 4047 Aluminum Welding Electrodes Aluminium Welding Rods Arc Welding Stick Supplier

Short Description:

For arc welding aluminums alloyed with copper, silicon, and magnesium


Product Detail

Product Tags

EN 573-3: E AlSi12

DIN 1732: EL-Al Si12

FEATURES & APPLICATIONS:

For arc welding aluminums alloyed with copper, silicon, and magnesium.

Also excellent for joining dissimilar grades of aluminum.

12% Silicon aluminum arc welding electrode with exclusive self lifting slag. Other aluminum grades such as Al 99, Al Mn, etc. are also available.

Unique self lifting slag.

Pure white long shelf life extruded flux coating outlasts conventional products in moisture resistance.
Can be manufactured in a variety of custom colors.

Available in hermetically sealed PURE ALUMINUM pull ring cans or vacuum packed foil bags for extended shelf life.

Also available in TIG form as item code 6047, in MIG form as item code 7091 and as a bare.

TORCH BRAZING ALLOY AS ITEM CODE 2191:

All Weld Metal Analysis (Typical Weight %)
Flux Color: White or Custom Colors
12.1 .001 .15 .01 .003 .001
Si Cu Fe Mg Mn Zn
Welding Current & Instructions
Recommended Current: DC Reverse (+)
Diameter (mm) 3/32 (2.5) 1/8 (3.25)
Minimum Amperage 50 70
Maximum Amperage 80 120

Welding Techniques: Start by using the upper portion of the amperage range. Feed the electrode quickly and move fast maintaining a very close arc gap.
Welding Positions: Flat, Horizontal

DEPOSITION RATES:

Diameter(mm) Length(mm) Weldmetal/Electrode Electrodes per lb (kg) of Weldmetal Arc Time of Deposition min/lb (kg) Amperage Settings RecoveryRate
3/32 (2.5) 14″(350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

APPROXIMATE ELECTRODE PACKAGING & DIMENSIONS:

3/32 (2.5) 1/8 (3.25)
Length (mm) 14″ (350) 14″ (350)
Electrodes / lb 49 33
Electrodes / kg 108 73