AWS Classification:AWS 5.9

DESCRIPTION:

Stainless steel welding wire has high cladding efficiency, good welding technical performance in all-position welding. They are widely used in industry: building structure, vehicle, bridge engineering, mining machinery, railway, oil pipe, gas pressure-bearing equipment, power equiment, etc.

MODEL NO. & SIZE:

1. Factory supply OEM service.

2. Model : ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi etc.

3. MIG wire size: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4.TIG wire size: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm .

INTRODUCTION:

We provide different kinds of stainless steel welding wire, including Mig solid welding wire, Tig rod welding wire and submerged-arc welding wire, all of high quality and are sold worldwide.

Except for 308 and 309, we also offer 304, 321, 347, 316L, 310, 2209, and 201. As well as special specifications such as 318L, 904L, 2594, NiCrMo-3, Ni1.

PACKING:

Mig welding wire packing (spool and drum pack)

Diameter: 0.8 - 2.0mm

Package:1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum

Tig rod welding wire packing (plastic tube)

Diameter: 1.0 - 5.0mm

Package: 5 kg/pack

Submerged arc welding wire

Diameter: 2.5 - 5.0mm

Package: 20kg/pack, 25 kg/pack

Neutral packaging and OEM are welcome!

CHEMICAL COMPOSITIONS OF STAINLESS STEEL WELDING WIRE:

Model No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

MECHANICAL PROPERTIES OF WELDING WIRE:

Model No.

Tensile strength Rm(Mpa)

Yield strength Rel or Rp0.2(Mpa)

Elongation

(%)

Model No.

Tensile strength Rm(Mpa)

Yield strength Rel or Rp0.2(Mpa)

Elongation

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

TIG and MIG stainless steel welding wire composition

YB5092-2005

AWS

Chemical Composition %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.


  • Previous:
  • Next: