AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 Flux-cored Welding Wire

Short Description:

AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 Flux-cored (FCAW-G) Wire is designed for high strength, low-alloy applications using 100% CO2 shielding gas.


Product Detail

Product Tags

AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 Flux-cored (FCAW-G) Wire is designed for high strength, low-alloy applications using 100% CO2 shielding gas.

Features
Capable of producing weld deposits with impact toughness exceeding 88 – 123 J (65 – 91 ft·lbf) at -40°C (-40°F)
Designed for welding with 100% CO2 shielding gas
Premium arc performance and bead appearance
Meets AWS D1.8 seismic lot waiver requirements
foil bag packaging

CONFORMANCES  SPECIFICATION  CLASSIFICATION
AWS AWS A5.29 E81T1-Ni1C-JH4
AWS AWS A5.36 E81T1-C1 A4-Ni1-H4
ABS ABS- Part2 4YQ460SA H5
CWB CSA W48 E551T1-C1A4-Ni1-H4 (E551T1-Ni1C-JH4)
DNV-GL DNV-2.9 IV Y46MS H5
LR LR – Chapter 11 4Y46S H5

DEPOSIT COMPOSITION

Classification Shielding Gas Polarity %B %C %Cr %Mn %Mo %Ni %P %S %SI %V Diffusible Hydrogen
mL/100g Weld Metal
E81T1-Ni1C-JH4 100% CO2 DC+   0.12 max. 0.15 max. 1.5 max. 0.35 max. 0.8-1.1 0.03 max. 0.03 max. 0.8 max. 0.05 max. 4.0 max.
E81T1-C1A4-Ni1-H4 100% CO2 DC+   0.12 max. 0.15 max. 1.75 max. 0.35 max. 0.8-1.1 0.03 max. 0.03 max. 0.8 max. 0.05 max. 4 max.
Typical Result, As -welded 100% CO2 DC+ 0.0050-0.006 0.04-0.05 0.04-0.06 1.12-1.42 0.01 0.81-1 0.012 max. 0.01 max. 0.24-0.35 0.02- 0.03 1.7-3.2

NOTES
To estimate ESO, subtract 1/4 in. (6.0 mm) from CTWD.
NOTE 1: FEMA and AWS D1.8 structural steel seismic supplement test data can be found on this product at www.lincolnelectric.com.
NOTE 2: This product contains micro-alloying elements. Additional information available upon request.
Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.


  • Previous:
  • Next: