AWS E7014 Carbon Steel Welding Electrodes J501Fe Mild Steel Welding Rods

Short Description:

J501Fe (AWS E7014) is an iron powder and titanium oxide type covered electrode.


Product Detail

Product Tags

Carbon Steel Welding Electrode

J501Fe                                                         

GB/T E5014

AWS A5.1 E7014                                    

Description: J501Fe is an iron powder and titanium oxide type covered electrode. It can be used for all-position welding with AC and DC, the deposition efficiency is about 110%.

Application: For carbon steel and low alloy steel structures, such as Q345 and other ships, vehicles and mechanical structures welding.

Chemical composition of weld metal(%):

C

Mn

Si

S

P

≤0.12  

≤1.25

≤0.60

≤0.035

≤0.035

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

0℃

Guaranteed

≥490

≥400

≥17

≥27

Tested

520 ~ 580

≥410

17 ~ 26

50 ~ 100

 

 X-ray inspection:  II grade

Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Welding current

(A)

40 ~ 70

70 ~ 90

90 ~ 130

160 ~ 210

210 ~ 250

260 ~ 310

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 