AWS E316-15 Stainless Steel Welding Electrode Arc Welding Rods for Manual Welding

Short Description:

A207 (AWS E316-15) is a low-carbon Cr18Ni12Mo2 stainless steel electrode with low-hydrogen sodium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A207                                      

GB/T E316-15

AWS E316-15

Description: A207 is a low-carbon Cr18Ni12Mo2 stainless steel electrode with low-hydrogen sodium coating.  Use DCEP (direct current electrode positive) and can welded in all positions. Since the deposited metal contains molybdenum, it has great corrosion resistance, heat resistance and crack resistance, especially good for resisting chloride ion pitting corrosion.

Application: Used for welding low-carbon 06Cr17Ni12Mo2 stainless steel structures, as well as high-chromium steels (such as Cr13, Cr17, etc.) that require no heat treatment after welding, and welding of dissimilar steels.

 

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Elongation

%

Guaranteed

≥520

≥30

 

Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 Notice:

  1. The electrode must be baked for 1 hour at around 250℃ before welding operation. Do not bake  repeatedly.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.