AWS E310T1-1/4 Stainless Steel Flux-cored Welding Wire

Short Description:

E310T1-1/4 is a gas shielded flux-cored wire designed for “all-position” welding and can be used with 75%Ar / 25%CO2 or 100% CO2 shielding gas.


Product Detail

Product Tags

E310T1-1/4 FLUX-CORED WIRE

CLASSIFICATION
AWS 5.22 Class E310T1-1/4 / ASME SFA A5.22 Class E310T1-1/4
UNS W31031 A#9 F#6

DESCRIPTION
E310T1-1/4 is a gas shielded flux-cored wire designed for “all-position” welding and can be used with 75%Ar / 25%CO2 or 100% CO2 shielding gas.
Welding parameters must be optimized to avoid hot cracking.

APPLICATIONS
E310T1-1/4 is most often used for welding base metals of similar compositions such as AISI 310 steels.
E310T1-1/4 can be used for welding carbon steel to stainless steel.
E310T1-1/4 can be used for welding or repairing high alloy heads and corrosion resistant castings of the same general composition.
Use low heat input – Suggest 30,000 Joules/In Maximum.
Avoid concave weld beads
Keep interpass temperature under 250°F
Fill all start and stop craters to avoid crater cracks.

TYPICAL CHEMISTRY (%)

C Cr Ni Mo Mn Si P S Cu
.10 25.9 20.4 .10 1.4 .82 .015 .005 .08

TYPICAL MECHANICAL PROPERTIES

TENSILE STRENGTH 89,000 PSI
ELONGATION IN 2” 38%
HEAT TREATMENT NONE

Note: Mechanical properties shown using 100% CO2

OPTIMUM TYPICAL WELDING PARAMETERS (using 100% CO2)

.045” DIA. FLAT & VERTICAL FLAT ONLY
AMPS 130-190 120-250
VOLTS 24-29 25-29
WFS (IPM) 225-450 200-600

NOTE: Stick out 3/8”-1/2”
Lower volts by 2 when using 75%Ar / 25%CO2

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.