AWS Class E308HT1-1/T1-4 Flux Core Wire Stainless Steel Flux-cored Welding Wire

Short Description:

AWS E308HT1-1/T1-4 Flux Core Wire Application & uses: Hardware tools. Metallurgy. Machinery. Construction. Shipbuilding. Petroleum. Chemical plant. Power sector. Gas Industry.


Product Detail

Product Tags

AWS Class E308HT1-1/T1-4 Flux Core Wire Specification

Classification AWS A5.22, E308HT1-1/T1-4
Form Welding Flux Core Wire
Type Of Welding Gas Shielded
Diameters .045”, 1/16”
Shielding Gas 100% CO2, 75-80% Ar/ balance CO2, 35-50 cfh
Welding Positions All positions
AWS E308HT1-1/T1-4 Flux Core Wire Application & uses Hardware tools
Metallurgy
Machinery
Construction
Shipbuilding
Petroleum
Chemical plant
Power sector
Gas Industry

AWS Class E308HT1-1/T1-4 Flux Core Wire Chemical Composition

C Cr Ni Mo Mn Si P S Cu
0.04 18.0-21.0 9.0-11.0 0.75 0.5-2.5 1.0 0.04 0.03 0.75

AWS Class E308HT1-1/T1-4 Flux Core Wire Mechanical Properties

Tensile Strength, kpsi: 75 min
Yield Strength, kpsi: *NS
Elongation %: 30 min

AWS Class E308HT1-1/T1-4 Flux Core Wire Parameters

Diameter Process Volt Amps Shielding Gas
in (mm)
 .035  (.9) GMAW   26-27 150-165 100%CO2
 .045  (1.14) GMAW  26-28 160-200 100%CO2
 .063  (1.6) GMAW  27-28 215-250 100%CO2

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.