AWS A5.4 E310-16 Stainless Steel Welding Electrodes Welding Stick Welding Materials

Short Description:

A402 (AWS E310-16)  is a Cr26Ni21 pure austenitic stainless steel electrode with titanium calcium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A402                                   

GB/T E310-16

AWS A5.4 E310-16

 Description: A402 is a Cr26Ni21 pure austenitic stainless steel electrode with titanium calcium coating. It can be used for both AC and DC with excellent operating performance. The deposited metal has good oxidation resistance under the high temperature condition of 900 ~ 1100 ℃.

Application: Used for welding the same type of heat-resistant stainless steel working under high temperature conditions, and can also be used for welding of hardened chromium steels (such as Cr5Mo, Cr9Mo, Cr13 and Cr28, etc.) and dissimilar steels.

 

 

 Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

0.08 ~ 0.20

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

≤0.75

≤0.030

≤0.030

 

 

Mechanical properties of weld metal:

Test item

 Tensile strength

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

 Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

 

Notice:

  1. The electrode must be baked for 1 hour at around 250℃ before the welding operation;
  2. Because the penetration depth is shallow during AC welding, the DC power supply should be used as much as possible to get deeper penetration. and the current should not be too large to avoid the redness of the welding rod.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 