AWS A5.4 E309-15 Stainless Steel Electrodes for Arc Manual Stick Welding, Welding Consumables

Short Description:

A302 (AWS E309-15) is a Cr23Ni13 stainless steel electrode with low hydrogen sodium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A307                                      

GB/T E309-15

AWS A5.4 E309-15

Description: A302 is a Cr23Ni13 stainless steel electrode with low hydrogen sodium coating. Use DCEP (direct current electrode positive) and can welded in all positions. The deposited metal has good crack resistance and oxidation resistance.

Application: Used for welding the same type of stainless steel, special-shaped steel, high chromium steel, high manganese steel, etc.

  

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

 Mechanical properties of weld metal:

Test item

 

Tensile strength

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

 Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Notice:

The electrode must be baked for 1 hour at around 150℃ before welding operation.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.