AWS A5.20 E70T-7 Flux Cored Arc Welding Electrodes Flux Core Welding Wire

Short Description:

AWS A5.20 E70T-7 Flux Cored Arc Welding Wire is a self-shielded flux cored wire designed for high penetration welding. It is suitable for flat, horizontal and downhill positions on DCEN polarity.


Product Detail

Product Tags

EN ISO 17632-A-T 42 ZW N 3

Characteristics and Application
AWS A5.20 E70T-7 Flux Cored Arc Welding Wire is a self-shielded flux cored wire designed for high penetration welding. It is suitable for flat, horizontal and downhill positions on DCEN polarity. Excellent performance on X-ray inspection, and desulfuration reduces cracking in welding thick plates, constrained joints and medium-carbon steel. The typical
applications are general fabrication and structural weldment where high deposition with good penetration and I or fast travel speed is needed. Available positions are flat weld, horizontal weld and vertical down ones of welding for fllet weld and lap joint.

Typical chemical Composition of Weld Metal (%)
C 0.29   Mn 0.45   Si 0.10  P 0.010   S 0.005   AI 1.45

Typical Mechanical Properties of Weld Metal
Yield strength 453Mpa Tensile Strenght 600MPa Elongation 25%

Notes on usage:
1.DC(-) polarity is recommended.
2. when impact toughness of weld metal is essential.
3. Keep the product dry, while it is stored or delivered.

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.