AWS A5.17 EM12K Submerged Arc Welding Wire

Short Description:

EM12K submerged arc wire contains higher levels of carbon, manganese, and silicon than EL12.


Product Detail

Product Tags

EM12K Submerged Arc Welding Wire

AWS A5.17 Class EM12K
EM12K submerged arc wire contains higher levels of carbon, manganese, and silicon than EL12. The increased carbon content gives this wire greater tensile strength, while the increased manganese and silicon content yields improved deoxidation properties. EM12K will produce weld deposits with minimal porosity even over rust and mill scale that may be present on the base metal. This wire is primarily used for single pass butt and fillet welds on mild and low alloy steel plates up to 1/2” thick. More specific applications would include ASTM A537, A283, Grades A, B, or C. Since EM12K offers high strength/low porosity welds on many steel alloys, it is the most cost-efficient submerged arc wire to stock.

TYPICAL WELD METAL CHEMISTRY %

C 0.150
Mn 1.100
Si 0.250
P 0.017
S 0.024

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 